Title: Fabrication and Characterization of Graphene Oxide and Reduced Graphene Oxide On Mos2 Film for IR Detectors
Authors: Gartia, Anurag
Kar, Jyoti Prakash
Keywords: rGO
Hummer’s method
MoS2
XRD
Raman
Issue Date: May-2023
Citation: 8th Edition of International Conference on Nanotechnology for Better Living(ICNBL), NIT Srinagar, 25-29 May 2023
Abstract: In recent years, infrared detectors have been widely used in surveillance, medical diagnosis, remote sensing devices, defence, industrial automation, communication, astronomy, where the advance materials are required to enhance the device performance. Graphene has gained tremendous attention in the field of photonics and electronics because of its numerous outstanding properties like zero bandgap, exceptionally high crystal and electronic quality, high mechanical strength, and electrical conductivity. In the cutting edge of technology, the graphene oxide - molybdenum disulphide hybrid structures have drawn tremendous attention for the development of high efficiency IR detectors, where MoS2 film is used for generation of photoelectrons, and graphene oxide is used to enhance the carrier mobility. In this work, modified Hummer’s method is used for the fabrication of graphene oxide (GO), where reduced graphene oxide (rGO) is obtained by the thermal reduction of GO at 350 °C for 1 hour. The appearance of XRD peak, corresponding to (001) and (002) peaks for GO and rGO, respectively confirms the crystalline nature of the materials. The characteristic Raman peaks of GO and rGO are observed at 1358 cm-1 and 1597 cm-1 , which correspond to the D bands and G bands, respectively. The layered structure of rGO is observed by Scanning electron microscope (SEM) technique. On the other hand, MoS2 film was grown by the sulphonation of sputtered Mo film on silicon substrate (p-type, 1-10 Ω.cm, 525 ± 20 μm). The characteristics XRD peak of MoS2 , corresponding to (002) plane, is observed around 2θ = 14.1° whereas Raman characteristic bands are observed at 386 cm-1 (E1 2g ) and 408 cm-1 (A1g ). Afterwards, rGO layer was deposited on MoS2 thin film. The. Post-deposition morphological and electrical properties of reduced graphene oxide and MoS2 thin film is carried out and co-related for next generation optoelectronic devices
Description: Copyright belongs to proceeding publisher
URI: http://hdl.handle.net/2080/4028
Appears in Collections:Conference Papers

Files in This Item:
File Description SizeFormat 
2023_ICNBL_AGartia_Fabrication.pdfPoster1.14 MBAdobe PDFView/Open    Request a copy


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.