dc.identifier.citationInternational Conference on Advances in Sustainable Solutions for Energy Transitions (ASSET), IIT Guwahati, 2-4 January 2025en_US
dc.identifier.urihttp://hdl.handle.net/2080/4996-
dc.descriptionCopyright belongs to the proceeding publisher.en_US
dc.description.abstractDoping depth profile measurement for Si is essential for determining junction depth, leakage current, threshold current, and overall device parameters. However, the widely used sophisticated approaches such as secondary ion mass spectroscopy and electrochemical capacitance-voltage (ECV) measurement are destructive techniques. Further, these techniques are not preferred for doping measurement of Si nanostructures, especially Si nanowires (SiNWs), due to complex multidimensional depth profiling. The work utilizes non-destructive majority-carrier depth profile analysis of the SiNW array using dry capacitance-voltage (CV) measurement and addresses the oxide layer and air-gap issues. A borondoped p-type SiNW array was fabricated by pre-optimized metal-assisted chemical etching. SiNW array was doped with P by spin-on-doping (spin-coating of P-containing phosphosilicate glass sol-gel followed by annealing), varying the P-concentration. P-concentration was varied in the sol-gel by varying the P2O5 concentration as 1.25 mM, 2.5 mM, 5.0 mM, and 7.5 mM. The Hall effect measurement estimates the surface carrier concentration as a reference for the differential CV measurement. The analysis estimates an effective doping depth and corresponding majority carrier concentration for the SiNW arrays with different doping concentrations. Due to the interstitial air gap formed by the SiNWs and the metal electrode, differential CV analysis overestimates the doping concentration and underestimates the doping depth. The differential CV analysis estimates the majority carrier concentration as 7.7 × 1026 cm-3 with an effective doping depth of 5.4 nm for the SiNW array doped with a P2O5 concentration of 5 mM.en_US
dc.subjectDifferential capacitance-voltageen_US
dc.subjectSpin-on-dopingen_US
dc.subjectEffective doping depthen_US
dc.subjectInterstitial airgapsen_US
dc.titleAnalysis of Capacitance-Voltage Measurements for Majority carrier Depth Profiling of Phosphorus-doped Si nanowireen_US
dc.typePresentationen_US
Appears in Collections:Conference Papers

Files in This Item:
File Description SizeFormat 
2025_ASSET_SPMuduli_Analysis.pdfPresentation834.91 kBAdobe PDFView/Open    Request a copy


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.