Please use this identifier to cite or link to this item: http://hdl.handle.net/2080/4805
Full metadata record
DC FieldValueLanguage
dc.contributor.authorKumar, Abinash-
dc.contributor.authorMazumder, R-
dc.date.accessioned2024-12-10T12:37:28Z-
dc.date.available2024-12-10T12:37:28Z-
dc.date.issued2024-11-
dc.identifier.citationInternational Conference on Advanced Ceramics for Sustainability (CERA4S), IIT Madras, India, 28-30 November 2024en_US
dc.identifier.urihttp://hdl.handle.net/2080/4805-
dc.descriptionCopyright belongs to proceeding publisheren_US
dc.description.abstractPiezoelectric ceramics are widely used as actuator, resonator, spark igniter and energy harvesting applications. Lead-free (Ba0.85Ca0.15)(Zr0.1Ti0.9)O3 (BCZT) piezoelectric have garnered immense interest due to their excellent dielectric and piezoelectric properties. However, the conventional sintering process for BCZT requires a high temperature of ~ 1500oC, which results in significant energy consumption. Recently, the cold sintering process (CSP) has emerged as a promising alternative, enabling the densification of ceramics at significantly reduced temperatures. However, there are no reports available on the cold sintering of BCZT ceramics. This study aims to investigate the factors affecting the cold sintering process of BCZT lead-free piezoelectric ceramics, focusing on flux concentration, dwell time, and sintering temperature. Here, Ba(OH)2 8H2O flux was used as a transient liquid phase and found that a concentration of 20 wt% provided the highest density, achieving a relative density of 86%. Furthermore, the sintering temperature and dwell time variation were also studied, and it was found that the effective sintering temperature was 250°C, and the dwell time was 1 hour. To further improve the density of the samples, annealing was performed at 1000°C and 1100°C, achieving a relative density of 90%. The dielectric behaviour with temperature of the cold-sintered and post-annealed BCZT samples was also characterized, revealing a dielectric constant in the cold-sintered ceramics without noticeable dielectric anomalies that generally marks the ferroelectric to paraelectric transition. After annealing, a hump indicating the Curie transition of BCZT became apparent, evolving into a broad transition peak around 90oC for annealed sample. Moreover, the annealed samples showed well-defined ferroelectric hysteresis loops, having a remanent polarization of 3.1 µC/cm2 and d33 value of 127 pC/N.en_US
dc.subjectCold Sinteringen_US
dc.subjectFerroelectricen_US
dc.subjectDielectric propertiesen_US
dc.subjectBCZTen_US
dc.titleMicrostructure, Dielectric and Piezoelectric Properties of Cold Sintered Lead-free (Ba0.85Ca0.15)(Zr0.1Ti0.9)O3 Ceramicen_US
dc.typePresentationen_US
Appears in Collections:Conference Papers

Files in This Item:
File Description SizeFormat 
2024_Cera4s_Akumar_Microstructure.pdfPoster2.67 MBAdobe PDFView/Open    Request a copy


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.