DC Field | Value | Language |
---|---|---|
dc.contributor.author | Basu, B | - |
dc.contributor.author | Venkateswaran, T | - |
dc.contributor.author | Sarkar, D | - |
dc.date.accessioned | 2005-12-29T09:18:36Z | - |
dc.date.available | 2005-12-29T09:18:36Z | - |
dc.date.issued | 2005 | - |
dc.identifier.citation | Journal of the European Ceramic Society, Vol 25, Iss 9, P 1603-1610 | en |
dc.identifier.uri | http://hdl.handle.net/2080/188 | - |
dc.description | Copyright for this article belongs to Elsevier Science Ltd http://dx.doi.org/10.1016/j.jeurceramsoc.2004.05.021 | en |
dc.description.abstract | In a recent work [Basu, B., Lee, J. H. and Kim, D. Y., Development of WC-ZrO2 nanocomposites by spark plasma sintering. J. Am. Ceram. Soc. 2004 87(2), 317–319], the processing of ultrahard WC–ZrO2 nanocomposites using spark plasma sintering is reported. In the present work, we investigate the processing and properties of WC–6 wt.% ZrO2 composites, densified by pressureless sintering route. The densification of the WC–ZrO2 composites was performed in the temperature range of 1500–1700 °C with varying time (1–3 h) in vacuum. The experimental results indicate that significantly high hardness of 22–23 GPa and moderate fracture toughness of 5 MPa m1/2 can be obtained with 2 mol% Y–stabilized ZrO2 sinter-additive, sintered at 1600 °C for 3 h. Furthermore, the friction and wear behavior of optimized WC–ZrO2 composite is investigated on a fretting mode I wear tester. The tribological results reveal that a moderate coefficient of friction in the range from 0.15 to 0.5 can be achieved with the optimised composite. A transition in friction and wear with load is noted. The dominant mechanisms of material removal are tribochemical wear and spalling of tribolayer | en |
dc.format.extent | 761394 bytes | - |
dc.format.mimetype | application/pdf | - |
dc.language.iso | en | - |
dc.publisher | Elsevier | en |
dc.subject | Sintering | en |
dc.subject | Tribochemical wear | en |
dc.subject | WC; ZrO9(sub)2 | en |
dc.subject | Wear | en |
dc.subject | Friction | en |
dc.title | Pressureless sintering and tribological properties of WC–ZrO2 composites | en |
dc.type | Article | en |
Appears in Collections: | Journal Articles |
Files in This Item:
File | Description | Size | Format | |
---|---|---|---|---|
sarkar2.pdf | 743.55 kB | Adobe PDF | View/Open |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.